Comment by Norm Stuart on February 2, 2015 at 12:57pm

Fast cooling being best for Zinc Crystalline glazes can be easily seen in this test tile:

fired to Cone 6 with a slow-cool with a few intricate crystals having formed;

then refired to Cone 04 without a slow cool and the entire glaze becomes crystallized without macrocrystals.

To live up to the name of Macrocrystalline Blue requires a third unspecified approach. But we don't have the kiln time to devote to that at our studio.

109.0% Macrcrystalline Blue ^6
52.0% Ferro Frit 3110
24.0% Zinc Oxide
24.0% Silica
2.0% Lithium Carbonate
6.0% Nickel Carbonate
1.0% Red Iron Oxide

Stars
Comment by Jeff Poulter on February 2, 2015 at 11:20am

I had a load of ornaments come out on Sunday that had little to no crystals on them.  The only difference was that I fired the underglaze on them to ^5 to harden it a little so the moly glaze wouldn't eat it so bad, but I'm guessing that I didn't get enough moly glaze on them since the surface was less porous.  I'll re-heat them & re-dip them and fire them again to see how they come out.  jhp


Stars
Comment by Jeff Poulter on February 2, 2015 at 11:15am

Actually I am finding that its not long holds like for Zinc-crystalline.  It's all about the surface tension and keeping the moly inside the kiln to re-deposit back on the surface.  They seem to grow pretty fast.  Of course I haven't gotten them as big as zinc ones either.  jhp


Stars
Comment by Norm Stuart on January 30, 2015 at 7:14pm

You have to cool very slowly to get glaze defects that interesting.

Comment by kees staps on January 30, 2015 at 5:58pm

Very nice but how is it done please

Kees


Stars
Comment by Denice E. Demuth on November 21, 2013 at 6:03am

Very cool, I hope your underglaze tests work.  Denice


Stars
Comment by Jeff Poulter on November 20, 2013 at 4:48pm

New Moly test.  Finally got my spiny starfish crystals.  Now to change the underglaze & hope I can still keep them & make them "POP".....  jhp

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service