Atmospheric effects on my first full load to be single fired.
Combination of C Harris Temoku and Variegated Slate Blue over Nutmeg.
On Laguna #80 medium brown clay
Tags:
Albums: Single Fire Success Story
Comment
Thanks, George. I have never used a sprayer. Learning to use one will take some practice.
Spraying interiors is not practical except on open forms like bowls and plates. Spraying inside of tall forms just gets you a lot of glaze right back in your face, and near uncontrollable thickness.
Best to pour in, pour out, and wipe the rim -- all as expeditiously as possible on raw ware.
Those are stunning. Did you spray the liner, too?
george,
this is still one of my fav's with the layering over nutmeg!
was looking at your two mugs george and was interested whether the liner here was nutmeg,,,,, not sure how to reference a pot
cp
I use white stoneware exclusively for a period of time, and then clean up and use a darker stoneware. I'll be switching back to brown in a week or two, and work with it until I use up my supply of 150 pounds.
great Yin and Yang mugs. this pot was a year old approximately , but i notice on brown clay. Are you able to keep brown and white in the same studio ? Or have you changed ?
cp
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2026 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics