Views: 149

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by juli long on September 27, 2013 at 7:48am

Brian, thanks for the crash course! Yes, I have Steven Hill's DVD and the setup to spray glazes, just haven't done it yet. I still have enough issues just with regular glazing to figure out. I am more impressed with your work. Thanks for sharing and keep up the great works!

juli


Stars
Comment by Brian Dean on September 27, 2013 at 6:51am

Juli, I do use Hanna's Fake Ash Glaze, but my Val Cushing G4 Glaze does use real wood ash. But it also uses Whiting (Calcium Carbonate) as well. Whiting is typically used in Fake Ash glazes. Real Ash glazes are typically used at Cone 10 as it normally requires the higher temperatures to flux and melt the ash and make it run. At Cone 6 you are not typically going to get the ash melt that you do at Cone 10 so you have to use something like Whiting which fluxes and melts at a lower temperature. If you want to know about the process of applying the layered glazes get your hands on the Surface Techniques of Steven Hill DVD. I pretty much spray all my glazes using small gravity feed detail spray guns which I bought on eBay and use with a small air compressor. Beyond that it is a matter of finding glazes that you like to use and which play well together when spraying and layering.


Stars
Comment by juli long on September 27, 2013 at 6:32am

Your work is really amazing.  I know zero about ash glazing and I dont think its something I will be doing, but I would be interested in the process of applying theses glazes and a little about the science behind it. Why do folks use a fake ash glaze instead of a real ash glaze? Just hoping to become a little more informed, because I am definitely becoming a fan!

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service