Once fired ^7 bmix ^5 clay body. Modified Steven Hill glazes. Strontium Crystal Magic for warm, Apricot, Baily's Orange, Copper Ash, Juicy Fruit with Iron and 2D Blue in different layers.

Views: 357

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by H. Louden Kiracofe on July 31, 2012 at 8:42am
Where canI find the recipe for S. H. Copper ash? I don't see the effect of 2-D blue inthe photo?

Stars
Comment by Don Olliff on July 24, 2012 at 3:48pm

Brian,

I will be doing some testing to see how stable these glazes are in the near future. I don't expect it to be a problem. I may be adding a little more glass formers if I intend to use these for functional pieces. Thanks for the nice comments.


Stars
Comment by Donna Ferrara on July 24, 2012 at 1:21pm

Beautiful!


Stars
Comment by Jan Wallace on July 24, 2012 at 2:27am

Stunning piece! Thanks for sharing how it was achieved too.


Stars
Comment by Denice E. Demuth on July 23, 2012 at 6:51am

Nice glaze layering clicking on full view made a  huge difference in color.   Denice

Comment by George Lewter on July 22, 2012 at 8:40pm

I like the separation effect in the white. It's like a miniature version of the rivulets seen in ash glazes.


Stars
Comment by Don Olliff on July 22, 2012 at 8:01pm

Sprayed the whole pieces with an airbrush using SCM warm. The next layer was Apricot on the outside with a thicker layer on the lip area. Some over spray went inside too. Next I used Bailey's Orange on the outside concentrating on the middle area. SH Copper Ash on the upper an lower areas outside leaving the middle alone but spraying some in the inside bottom section. Juicy Fruit with iron was next covering most of the bowl including some overspray inside. Finally used 2D Blue with a heavy layer on the upper section, inside bottom and on the lip area as well as the bottom foot area.


Stars
Comment by Don Olliff on July 22, 2012 at 5:59pm

The color is not right on this image. click on "View Full Size" to see a better representation of the glaze colors.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service