Comment by Joan Hendershot on December 21, 2013 at 9:38am
Thank you so much John for sharing

Stars
Comment by John McClure on December 20, 2013 at 7:31am

Glad to share, I use Richard Bush’s Nutmeg, Butter Yellow (source unknown) and Pete Pinnell’s Strontium Matte (aka Weathered Green Bronze). I’ll include the recipe for Butter Yellow at the end, but the others are so widely available I have chosen to not repeat them here.  I mask the bisque tumbler and apply Nutmeg, then remove the masking, next apply Butter Yellow.  Once the glazes are dry enough to handle I hand apply Strontium Matte.  So the result is a flowing glaze where Nutmeg and Butter Yellow combine and stiffness with the Strontium Matte.  Be careful in glazing and use a thin Butter Yellow.  If the glazes are too thick you'll be cleaning your shelf.

Butter Yellow

Kaolin-EPK            20.0

Feldspar-Potash    32.8

Silica                      14.5

Whiting                   14.5

Zinc Oxide              14.5

Lithium Carbonate    3.7

Add

Rutile                        5.0

Tin Oxide                  5.0


Stars
Comment by Joan Hendershot on December 19, 2013 at 6:26pm
I love your tumblers, can you share what glazes you used?

Stars
Comment by John McClure on December 17, 2013 at 8:51pm

Thanks


Stars
Comment by juli long on December 17, 2013 at 5:50pm

Cool glaze combo!

juli

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service