Comment by Keiko Stusnick on May 5, 2013 at 4:01pm
Voila!
Linda Christianson's Shino cone 4 to cone 14 (red or ox)
F4 F S. 42.3
Spodumene. 35
EPK. 5.9
Soda Ash. 9.4
Neph Sy. 3.5
Ball clay. 3.5 (I used OM 4). Add 2% Bentonite
------------------------------
99.6 (weight-wise)
I won't guarantee. My vase (cone 6 ox) got freaky particles, but it didn't leak fortunately. A similar way happened for Warren Mackenzie Shino at salt-woodfiring. I don't know if it was caused by temperature. Please do test tile first. Good luck!

Stars
Comment by Denice E. Demuth on May 5, 2013 at 9:30am

Yes posting that glaze would be nice I'm sure I am not the only one who would like it.  Denice


Stars
Comment by Keiko Stusnick on May 4, 2013 at 6:56pm
Thank you, Denice! No, I don't call this a Liner glaze. It's Shino for cone 4 through cone 10 (red and ox). Linda Christianson introduced me this recipe. Would you like to have it?Sometimes the glaze will come off like a powder, but this didn't have any problem. Maybe the higher the temp, the better. I did this with cone 6. Inside and outside have the same 'shino' glaze.

Stars
Comment by Denice E. Demuth on May 4, 2013 at 2:17pm

I like the free flowing brush work and the organic style of the mug.  Do these have a liner glaze on the inside?  Denice

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service