Comment by Jeff Poulter on May 28, 2014 at 7:44pm
My favorite part is the lid. I think spraying would do the trick as long as you got the thickness right when spraying. jhp

Stars
Comment by Jeff Poulter on May 28, 2014 at 7:41pm
Hi Liz
Which Tenmoku recipe are you using? I tried using CHarris Tenmoku with an ash nuke glaze over it. It worked on a test but not on the pot. I would try spraying it. Let me know. jhp
Comment by Liz Wolfe on May 28, 2014 at 7:27pm
This is an 18" high vase and lid. Made at MIY Studio in Hollywood, Fl. It is High Water clays earthen red cone 5. The pieces were bisque fired together then glaze fired in the same kiln (but the lid was not on) by Erik Evans. I put a light coat of tenmuko on the vase and waxed tall waxy shapes on the bottom of vase, then sprayed tenmuko again. I spayed the lid at this time. (The waxed part came out black.) Let dry. Masked off the bottom and sprayed Hannah's fake ash on the shoulder of the vase and the whole lid. Painted the fake ash as drip shapes from the top where the spray of fake ash ended into the middle. The lid and the shoulders of the vase came out very different colors even though they were glazed and fired at the same time. The lid is maroon and the shoulder of the vase is grey, black and red where it has crawled. I guess that the application of the fake ash was too thick on the shoulder of the vase. The part that I applied with a brush is grey and green. I applied several coats in a downward motion.

I like this glaze combo very much but I haven't mastered the application. I was going for the maroon color. I think that May be achieved with a thick coat of tenmoku and a thin coat of fake ash. I've gotten a variety of results with this glaze combo.

Stars
Comment by Jeff Poulter on May 28, 2014 at 3:51pm

Beauty!  I love the shadings and colors!  jhp

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service