Comment by Jeff Poulter on June 28, 2013 at 4:09pm
Hi Juli
If I get it started b4 8pm I can crack it by 7am and pull stuff out by 8:30. I'm looking for a replacement glaze that I get from Bath Potters. It is a low fire Speckle Blue that when I add moly to it and layer it I get the pots that you have seen me post. They don't make it anymore so I have been looking for a replacement. I read on someone's blog that the Show Saver can go from ^3 to ^10. That might make it a candidate for layering. In some of the pics I saw where they added colorants it already looked like some of the metallics were trying to crystallize. Moly is very fussy about crystallizing as it goes from a solid to vapor at about 700C. I'm trying to find the best elements and or glazes to hold it in the glaze structure so that the crystals grow. I don't know if the Moveable Feast would be fluxed enough at ^5-6 but I will try it. It is supposed to be an update of SS but it looks somewhat different. Since I know moly likes manganese I might try the 2 purple versions. I'm going to try for tomorrow. jhp

Stars
Comment by juli long on June 28, 2013 at 3:55pm

Jeff,

Boy you are quick with the results. Must have opened the kiln while it was on fire!D

Just wondering what color or effect you are after? I looked at the show saver glaze, but only saw reference to cone 10.


Stars
Comment by Jeff Poulter on June 28, 2013 at 12:45pm

OK, so the Ravenscrag did not like the moly, even with the low fire speckle over it.  It was better, but not acceptable.  I also made a test batch of any Alberta Black, but used Ohio Slip instead & it came out alright.  With the low fire speckle over it, it started segregating & allowing the moly crystals to form.  This weekend I will try Show Saver.  I read that it can fire from ^3-^10.  I wonder if Martins Moveable Feast has the same firing range?  It says it is an updated version of Show Saver, but there are quite a few changes.  Will let you know how it turns out.  jhp


Stars
Comment by Jeff Poulter on June 27, 2013 at 3:18pm

I think I will mix up a little test of the black & throw it in with the re-fire tonite.  I have the Ravenscrag & also Ohio slip.  Ohio slip is said to be a very close match to Albany.  There aren't many recipes on their sight for it, but on one they spray just the plain slip & fire it to ^6 & it looks like Albany slip.  i should test that as well.  jhp


Stars
Comment by juli long on June 27, 2013 at 3:10pm

Hey Jeff,

No, I haven't , but I want too. I ordered the Alberta slip before I knew I had to calcine it, otherwise I would have used the Ravenscrag. Lazy here too, and the bad thing is I have to do it all again when I make up another batch. ugh!


Stars
Comment by Jeff Poulter on June 27, 2013 at 3:00pm

Hi Juli,

    Just wondering if you have tried using Ravenscrag instead of Alberta?  I have seen recipes with 80% Ravenscrag & 20% FF3134 with various colorants & no calcining & wondered if they work as well.  I guess I am just lazy & didn't want to have to calcine ingredients.  I think I'll give the Glossy Black a try.  jhp


Stars
Comment by juli long on June 27, 2013 at 2:48pm

 Tony Hansens rutile blue glaze

40% Alberta slip

40% Alberta slip (calcined)

20% frit 3134

5% rutile    (I tested 4% and 5%) and I liked 5%

really three ingredients , you just have to put some of the alberta slip in bowls and fire it in your

kiln to make it calcined.  Tony had a great thread on this glaze here a few mt. back.  I tested it on all my clays.  I did not like it on my Armadillo cinco blanco clay.  This clay is Armadillo Cinco rojo,

It looks totally different on Bmix, and great on Trinity cone 6 clay.


Stars
Comment by Joe Shaw on June 27, 2013 at 12:34pm
Hi! Great looking pieces. I am looking for both green and blue satin (or high gloss) glazes that will work well with my firing schedule. The blue I am using tends to pin hole, especially if I do more than one high fire. Mind sharing this glaze? Thank you! Joe Shaw

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service