Comment by Denice E. Demuth on November 18, 2013 at 3:10pm

Nice glaze combination.   Denice


Stars
Comment by Norm Stuart on November 11, 2013 at 10:20pm

I wish I understood the mechanism of these gold/black colored manganese saturation glazes better.

Black Manganese Dioxide (MnO2), the primary component in dry cell batteries, decomposes into green Manganese Monoxide Mn(II)O, at 995 F.

Manganese, stripped of the oxygen in a reduction firing, would melt around cone 8. But Mn(II)O remains stable without evaporating until well above cone 12. In a glaze melt, Mn(II)O acts as a strong base - but is not a strong base or reactive at room temperature. It was one of the first natural pigments used in cave paintings and body decoration.

Somehow this green base compound combines with iron oxide, cobalt oxide, and copper oxide to create either matte black or reflective gold. Adding tin oxide makes the black blacker and the gold golder.

Sharply reduce the level of manganese to a level roughly equal to the level of the iron, cobalt and copper and the glaze color turns out silver.

Iron with Manganese alone forms a nice black glaze, while Tin with Manganese yields brown. Manganese Silicate without alumina is purple, as is Manganese with Cobalt.

What is the structure of these silver and gold reflecting compounds? Someone must know.  Not I.


Stars
Comment by Tim O'Neill on November 11, 2013 at 5:19pm

Hey George - This was the queen of the kiln.  I resorted to commercial glazes for this one.  It was fired to cone 6 in elctrick ox - Metallic Saturation glaze on rim that flowed into the Textured Turquoise over Blue Rutile  (Amaco Potter's Choice glazes) - The red band is chattered with a RIOX wash (no glaze).  I've been able to reproduce the results on a similar pot.  These glazes are very predictable once the palette is built.

Comment by George Lewter on November 11, 2013 at 5:06pm

What is that black glaze around the rim and inside. It has a nice satin sheen.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service