Comment by Denice E. Demuth on March 8, 2014 at 8:42pm

I'm not worried about the food safe aspect, I rarely make any thing that is used for food or drink.  I mostly work in tile, sculpture and pots.  If someone wants me to make them mugs or plates I'll use a purchased glaze that is food safe.  I am very cautious when it comes to safety, I have even been known to question a manufacturer about a glaze that has been labeled food safe that seems kind of iffy.    Denice


Stars
Comment by Robert Coyle on March 8, 2014 at 5:17pm

I keep forgetting to say this glaze was not tested as "food safe" but since I plate my pots with a copper solution in a sulfuric acid bath for at least 2 days, I don't think that lemon juice will effect it.


Stars
Comment by Denice E. Demuth on March 8, 2014 at 3:09pm

Thanks for posting that glaze, I'm going to be doing dome testing soon I plan to give it a try on the Laguna speckled buff and Flinthills buff.  Denice


Stars
Comment by Robert Coyle on March 7, 2014 at 9:02am

Note: taken from Glazes Cone 6 by M Bailey and modified

Glaze test on Laguna clay bodies. Fired up to cone 5 with kiln setter shut off. 125 F/hr from 1700f to shutoff.

Comp              %

Neph Sy          68

G.Borate         08

Ball Clay         08    

Whiting           05

Silica               04

Rutile             02

Titanium         02

Cobalt Carb     01

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service