These are all my very first tests using my new kiln!! All are cone 6 oxidation. I am pretty pleased. If you have any feedback or suggestions please let me know!! :D

Views: 133

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Amanda Sullivan on May 13, 2013 at 7:36pm

I have seen your tools they look very professional!! Good job!! And I like the chattering on that bowl, I can never get it to turn out right...


Stars
Comment by Robert Serva on May 13, 2013 at 6:34pm

Thanks, It was one of my first tries with chattering, I have made a bunch of tools and they are starting to work out real well. I get many variations depending on the tool material thickness and tip I grind on it. The Coyote Mottled blue is very reliable, it always gives me good results and seems to work well with a wide range of clays. 

Comment by Amanda Sullivan on May 12, 2013 at 7:26pm

Very nice bowl by the way!

Comment by Amanda Sullivan on May 12, 2013 at 7:25pm

Lol sorry That is Minnasota Clay Co. Iron Red With Coyote red gold on top


Stars
Comment by Robert Serva on May 12, 2013 at 7:19pm

I Use the Mottled Blue also and really like it. Here it is on brown Standard clay on this 10 inch bowl.


Stars
Comment by Carl Ray Crutchfield on May 12, 2013 at 3:04pm

:) the 4th one from the other left,  .... the brown one:)  I use coyote glazes also.  I buy clear and creamy matt and then add colorants to get the glazes i want to use, but I also use their premixed wet glazes for accents and brush work.  I don't really have the space to mix glaze from scratch. 

Comment by Amanda Sullivan on May 12, 2013 at 8:43am

I sent you a friend request!

Comment by Amanda Sullivan on May 12, 2013 at 8:41am

Thanks! Commercial.. I am going to start mixing my own soon.  It is Coyote Mottled blue with Mayco Alabaster on top


Stars
Comment by Carl Ray Crutchfield on May 12, 2013 at 7:26am

Well you should be please, very nice results.  Are they commercial glazes or mixed from recipe?  What is the test 4th from the left, please?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service