These are all my very first tests using my new kiln!! All are cone 6 oxidation. I am pretty pleased. If you have any feedback or suggestions please let me know!! :D

Views: 141

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Amanda Sullivan on May 17, 2013 at 9:33pm

Hey Sky Hibberd, the orange looking glaze is Coyote Shino with Mayco Alabaster over it. Thanks! Do you have a FB page? if so mine is www.facebook.com/sullivan55amanda

I am unable to add friends but feel free to add me, if not no worries!

Comment by Sky Hibberd on May 17, 2013 at 12:12pm

Hi Amanda, i FB you early today. I was Wondering what the 'Yummy' Orange Glaze is Called. Thank You 

Sky -H-


Stars
Comment by Troy Bungart on May 12, 2013 at 3:28pm

The orange one is just yummy!

Comment by Amanda Sullivan on May 11, 2013 at 6:45pm

Its true! Just a little scared!

Comment by Amanda Sullivan on May 11, 2013 at 6:24pm

these are made on a wheel just open bottomed and wide then pull up a wall and keep clay as a catcher on both sides.  Or you can make slabs cut them into rectangles and sit them up kind of like an L shape.  And Thank you! That is all I have done so far with my kiln also is tests... Im scared to do a load of work that I have been working on for a couple of months


Stars
Comment by scott kelly on May 11, 2013 at 2:59pm

Did you make those pcs, cut up from a pot? I'm not sure what I'm going to use. I have done no test yet.


Stars
Comment by scott kelly on May 11, 2013 at 2:48pm

Claps hands!  New Kiln?  ya....... I have a new one also. I have only done one test fire with it.

Those all look great by the way.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service