Probably. I haven't used this glaze in a long long time. It is a wonderful glaze but I lost interest in it. 


Stars
Comment by Tom Anderson on July 19, 2017 at 4:19pm
Nice work Joseph. Makes me wonder if I can get Redstone to fire into that color range?
Comment by Joseph Fireborn on July 19, 2017 at 9:55am

Henry, I slow cooled it drastically to get it the semi matte color. I also probably used a different red iron oxide than you. I used a synthetic RIO that has colorant in it. 

Hope this helps? 

Comment by Henry Pope on July 19, 2017 at 9:54am

Can you post your variation of this glaze?  I used it some time ago but could never get it to loo like the reddish semil-matt glaze in the original article.  So I found another  similar glaze, bird's matt white, yellow, and red variations, from an earlier Clay Times article (^6 ox).  Would like to know how you got Bush's glaze to come out as seen in your postings.  Thanks - Mikpo Pottery

Comment by Daniel Ramos speak-spanish. on December 23, 2015 at 6:42am
thanks
Comment by Joseph Fireborn on December 23, 2015 at 6:37am
Comment by Daniel Ramos speak-spanish. on December 23, 2015 at 6:35am
Please could write the recipe of Richard Bush or a link to where to look , thanks
Comment by Joseph Fireborn on August 31, 2015 at 7:09am

See George's comment below. It is a variation of Richard Busch's recipe, with my 15 hour cone 6 schedule.

The brush marks are a RIO stain, 50 GBorate and 50 RIO. I don't usually use Grestley Borate, but I don't mind on stains as I like it nice and thick because I can just dip my brush in water to adjust the thickness.


Stars
Comment by Denice E. Demuth on August 31, 2015 at 6:50am

This glaze looks familiar but I can't quite place it.  Did you use ROI and frit mix and brush it on bisque to get the darker section on the Yunomi.   Denice

Comment by Joseph Fireborn on August 29, 2015 at 5:09am

Very good! Yes it is his glaze combination. Although I used iron stain instead of the MnO based stain. I have the ingredients for it, but I am not sure if it is worth the difference in color. I might mix up some eventually.

I am loving the glaze combination because my true heart wants to do woodfired, but I can't due to the location I live. So I will just continue to use these and adapt other colors in with it. This is probably my most favorite piece I have made to date.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service