jugs, pitchers

Views: 149

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Daniel Ramos speak-spanish. on April 20, 2015 at 9:39pm

Esta bellísimo el color amarillo a café rojizo 

Comment by Joan Scott on December 8, 2013 at 3:12pm

Thanks Karen and Juli

Comment by Karen on December 7, 2013 at 7:07pm

These are awesome!

Comment by juli long on December 7, 2013 at 5:50pm

So toasty warm!!

Comment by Randy McCall on December 7, 2013 at 3:20pm

Thanks I will try it the next time I fire.

Comment by Joan Scott on December 7, 2013 at 12:28pm

Hi Randy,

I posted this info on Ash Glazes quite some time ago. I am pasting what I wrote to Mike at that time. There is other interesting info there if you look up the tread. Here is what I answered at that time. 

Permalink Reply by Joan Scott on January 6, 2012 at 8:08pmDelete

Hi Mike,

I have dug out the original old recipe from The Craft of the Potter (Michael Casson UK potter extraordinaire, sadly passed away). He fired high temp but I liked the dry ash texture and tried to lower the temp. 

Original Recipe

Ash          50

Ball Clay    25 

Kaolin       25

I don't know if he washed his wood ash, I don't. What I do is put it thru window screening ridding of big chunks and then put it thru 80 to 100 mesh. 

My starting recipe is:

Ash                        23

Whiting                   16

Feldspar

or Nepheline Syenite  13

Ball                         48

Iron oxide                 5 / 10

Bentonite                  2

Then I test it and usually I have to tweak it to my liking (more flux perhaps). I fire higher than 6 more in the cone 7 range and hold it for 30 min at high temp. I have also played with firing down at 1800F to 1600F holding it at 1700  for awhile.  Leaving out the iron oxide to work with the base and adding other possible oxides could be pursued of course. It is a glaze that works best on outside of functional ware with a liner glaze on inside. Hope there is something here for you.

Comment by Randy McCall on December 6, 2013 at 4:53am

Joan I am interested in your outside glaze.  Can you share it with us?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014