Potters & Sculptors - Making Rock from Mud
Comment
Esta bellísimo el color amarillo a café rojizo
Thanks Karen and Juli
These are awesome!
Thanks I will try it the next time I fire.
Hi Randy,
I posted this info on Ash Glazes quite some time ago. I am pasting what I wrote to Mike at that time. There is other interesting info there if you look up the tread. Here is what I answered at that time.
Permalink Reply by Joan Scott on January 6, 2012 at 8:08pmDelete
Hi Mike,
I have dug out the original old recipe from The Craft of the Potter (Michael Casson UK potter extraordinaire, sadly passed away). He fired high temp but I liked the dry ash texture and tried to lower the temp.
Original Recipe
Ash 50
Ball Clay 25
Kaolin 25
I don't know if he washed his wood ash, I don't. What I do is put it thru window screening ridding of big chunks and then put it thru 80 to 100 mesh.
My starting recipe is:
Ash 23
Whiting 16
Feldspar
or Nepheline Syenite 13
Ball 48
Iron oxide 5 / 10
Bentonite 2
Then I test it and usually I have to tweak it to my liking (more flux perhaps). I fire higher than 6 more in the cone 7 range and hold it for 30 min at high temp. I have also played with firing down at 1800F to 1600F holding it at 1700 for awhile. Leaving out the iron oxide to work with the base and adding other possible oxides could be pursued of course. It is a glaze that works best on outside of functional ware with a liner glaze on inside. Hope there is something here for you.
Joan I am interested in your outside glaze. Can you share it with us?
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2026 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!