Large stoneware fruit bowl with grape leaf and vine relief. Metallic green glaze.

Views: 265

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Tina Meschko on July 20, 2013 at 6:21pm

Okay guys, found it.It's actually a base recipe with color options. I included all.

METALLIC GREEN

This metallic luster glaze looks awesome on clays with iron - Laguna’s Electric Brown, Hawaiian and Standard’s 266 Brown or over engobes or stains made from red iron oxide.Both the Sky Blue and Ocean variations also produce metallic lusters and look best on iron rich clays, stains and engobes. Three brushed-on coats really cover well; if more translucency is desired, one heavy or two lighter coats do the trick.

 

BASIC RECIPE

  • Frit 3269...........27.0%
  • Laguna Borate.......15.0%
  • Spodumene..........40.0%
  • EPK............18.0%

                                 

 ADD:

  • Bentonite...........2.0%
  • Brushing Medium.......1.8% [add if brushing]

 

For green and blues see colorants below:

 

METALLIC GREEN

ADD Colorants:

  • Tin Oxide......... 6.8%
  • Copper Carbonate......4.8%

Using the basic recipe for Metallic Green above but changing colorants will give you these recipes

 

METALLIC SKY BLUE

ADD Colorants:

  • Tin Oxide..........6.8%
  • Copper Carbonate........3.0%
  • Cobalt Carbonate.......1.5%

 

METALLIC OCEAN

ADD Colorants:

  • Tin Oxide............7.0%
  • Copper Carbonate.........4.0%
  • Cobalt Carbonate......... 1.0%
Comment by juli long on July 20, 2013 at 5:57pm

count me in as well! I want to try this glaze *)

Comment by Robert Serva on July 20, 2013 at 4:29pm

post the recipe up...:)  It would be the first I try from scratch.

Thanks again

Comment by Darlene Shemanski on July 20, 2013 at 4:58am

Tina, I would love the recipe... email dshemanski@gmail.com

Thanks

Darlene

Comment by Tina Meschko on July 19, 2013 at 7:59pm

Thanks you for the kind comments. The hand-work is all clay, no wire. Darlene, I can tend to be detail oriented and enjoy getting lost in the sculpting work. The little coils are fine coils of clay rolled around a pencil. Set just 'til they can be handled. The glaze is one of my favorites which I make from a recipe, not pre-made. Willing to share.

Comment by Robert Serva on July 19, 2013 at 5:35pm

Yes, Outstanding!!  Is this glaze a commercial one or one from a recipe?

Comment by George Lewter on July 19, 2013 at 12:11pm

Beautifully done. Are the tiny coils clay or wire?

Comment by Darlene Shemanski on July 19, 2013 at 11:38am

Tina, I love this bowl. How on earth were you able to create such a delicate and intricate pattern? Is the glaze Floating Green from Mastering Cone 6 glazes?

Great work!

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014