Shellac technique on black clay with white glaze

Views: 151

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Susan Amann on June 12, 2017 at 5:30pm

Yes!  Oxidation fired to cone 6 using Standard Clay #266

Comment by Brenda Outram on June 12, 2017 at 5:23pm

Very nice, was it done in oxidation?

Comment by Susan Amann on June 12, 2017 at 5:21pm

Thank you Brenda!  This glaze is from Ceramics Monthly a while back.

White Satin Matt Glaze (Cone 6)

Gerstley Borate .............................. 31.63%

Talc ............................................... 13.95

Kona F-4 Feldspar .......................... 19.80

EPK (Edgar Plastic Kaolin) ............... 4.98

Silica (Flint) ..................................... 29.64

                                                  100.00%

Add: Zircopax ................................. 5.11%

Bentonite ............................... 1.99%

Comment by Brenda Outram on June 12, 2017 at 10:47am

Hi Susan, Beautiful vase, can I ask what glaze you're using, it breaks beautifully.

Comment by Susan Amann on April 2, 2012 at 6:23pm

Thank you Tony!


Stars
Comment by Troy Bungart on April 2, 2012 at 5:46pm

very nicely done.

Comment by Susan Amann on April 2, 2012 at 3:24pm

Hi Denice!  Thank you!  Yes it is similar to wax resist.  I apply the shellac to bone dry greenware.  After the shellac has dried, I take a damp sponge and wash away a few layers of the clay, which leaves the shellac portion raised.  Then bisque and glaze with a glaze that will highlight the raised surface areas.


Stars
Comment by Denice E. Demuth on April 2, 2012 at 2:34pm

Nice work what exactly is the shellac technique is it like wax resist.     Denice

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service