Band-aid solution #4 for crazing: Add silica to the clay body

It is not usually practical to adjust the body because most people use prepared clays. But if so, it is true that adding coarser sizes of high-expansion silica have the end-effect of compressing the glaze (because quartz particles contract 1% when going down through quartz inversion around 570C). Supposedly the added silica is not dissolving into the aluminum-silicate crystal body structure that the feldspar is creating and can impose its higher expansion on the surrounding matrix. Vitrified ceramics are brittle, does it sound good if individual silica particles are playing their own game, not expanding/contracting in harmony with their surroundings? Adding silica must be done at the expense of other materials in the recipe: If the clay component is reduced, the body will be less plastic; if the feldspar is cut vitrification is lost. This not only sacrifices strength but breeds another thermal expansion misfit: Cristobalite, a crystal phase of silica. Cristobalite suddenly expands/contracts on heat/cooling through 225°C, it actually develops within the body during firing when feldspar is lacking. Your firing and clay body may not be so scientifically balanced as all this, but it may still take a lot of silica to fix the crazing and temperature gradients that exist in firing bodies create expansion gradients that move like waves through the ware during cooling, causing dunting.

Views: 105

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service