Comment by Jan Wallace on December 5, 2011 at 1:02am

Thanks Patricia.

Comment by Patricia Bridges on December 4, 2011 at 5:20pm

Simple Stupid- I dip them - plunged into to bucket with my hand. Painted over the texture with a lighter glaze. These two glazes are a floating blue.

Comment by Jan Wallace on December 3, 2011 at 2:05am

I love these too Patricia. Can you explain please how you glazed these pieces ie dipped, sprayed, poured etc. Are the glazes you have used available on this site and if not, are they ones you would care to share at all? Thanks.

Comment by Patricia on December 2, 2011 at 2:10pm

Thanks. These are big sellers.  I call these Po' Boys, as they are the cheaper and simpler version of my larger trays/plates.The two longer ones are about 5 x 10 and sell for $25 for one $45 for two. I sell the smaller 5x7 for $20 and 2 for $35. My bigger versions have a beautiful foot and are much more sophisticated and sell for $75/$85.

Here is a link to the bigger ones.

http://www.blog.bridgespottery.com/2011/10/getting-to-know-shapes.html

Comment by rose maguire on December 2, 2011 at 1:08pm

Love what your doing with the textures Patricia but really love these plates. Do you sell these and how much for?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service