Potters & Sculptors - Making Rock from Mud
The dark glaze underneath breaks through.
Tags:
Comment
I think that you can get volcanic ash at just about any ceramic supply shop. I have gotten mine most recently from Bailey's.
My wife has been looking for a turquoise like this and such an effect. Nice piece. Where do you procure Volcanic Ash?
Yes Donna you'er right. I guess that I have tweaked this recipe around a bit and stopped taking it back to 100. The copper and tin are not in percents they are just a number.
Wonderful piece and glazing by the by
Since the glaze does not add up to 100% are you adding in a 106 gram recipe 10.6 tin and 6.36 copper or is the % really just treating the recipe as 100? I know that is an odd question but I am thinking the Bentonite and Magnesium got added after the fact in the recipe so the two colorant/opacifiers are as they are and not %. Curiousity running my mouth here.
Thank you Tony for the recipe. looks like fun. Happy firing.
I don't know where I got this glaze and I don't know how much I have changed it over the years. I am a pretty bad note keeper.
Cone 6 electric
Volcanic ash 82
Whiting 8.3
Lithium carbonate 7.6
Gerstley borate 2.1
Bentonite 1
Magnesium carbonate 5
add
6% Black copper carbonate
10% Tin
This is the blue green glaze over the Tenmoku style glaze which is breaking the surface like an oil spot glaze.
yes, could not agree more, one of the hardest things for me is to know when to stop glazing.
Thanks Carl,
Anyone can over work a pot disguising poor technique, I like to keep it simple. Sometimes the hardest thing to do is let a simple form be what it is.
gorgeous glaze effect and beautiful form.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014