So this was supposed to be a purple version. I had the blue for boys & now I have pink for girls. The top glaze is in the same family of glazes but the composition must be different. You never know with store bought glazes. Now I'm going to have to test them all to see what colors I can come up with. jhp
Hi Juli,
I used Cornwall Stone, but don't know if it is the real deal or made up stuff. The CS that I have is definitely somewhat coarse and not nearly as refined as most of the other materials I use. I definitely like what the glaze does and I think the CS has a lot to do with that. I'm sure also that the difference in rutiles will make a difference as well. jhp
Jeff, did you use cornwall stone as per recipe or did you substitute it? Love your glaze and thought I might make up a batch of "donna white".
This piece is amazing thank you for posting the additional details.
Searched for Donna's White on the site and cannot find it. Do you have a link please ?
Your effect is grand, and most amazing for an electric fired piece.
May i ask how tall the piece is ?
Wow Jeff!! Looks really great. Will you share your technique? This is two glazes layered? Did the glaze run off the foot of the vase?
-chantay
I have to give a lot of credit to Donna Ferrara as this is her Matt White Base with 4% rutile in it. After she posted it, i just kept going back to it & trying more layering tests. I think I will try her NWLS as well. It is a little different and we'll see what it does. jhp
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2026 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics