Clay bodies left to right: stoneware 55, speckled brownstone, Ellen buff, porcelain
Glazes front to back:
folk art guild white, Zam celadon, C Harris Tenmoku, strontium crystal magic cool, strontium crystal magic warm, SH red orange

Views: 235

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Daniel Ramos speak-spanish. on May 18, 2015 at 2:51pm

Gracias Norm, meteré unas pastillas de prueba  


Stars
Comment by Norm Stuart on May 18, 2015 at 1:59am

According to the chemistry, spodumene has only 20% of the ceramic-flux, lithium oxide, contained in lithium carbonate. The extra material is the equivalent of kaolin and silica, so these two ingredients in the recipe should be reduced to keep the chemistry identical.

But in this recipe "Weathered Bronze Green" the glaze I made using spodumene looks only slightly different than a glaze made with the same weight of lithium carbonate or lithium fluoride.

Chemistry of / Componentes químicos de:

Spodumene

Lithium Carbonate

Kaolin / Caolin

Según a la química, spodumene tiene sólo el 20% de la flujo-cerámica, óxido de litio, contenido en carbonato de litio. El material extra es el equivalente de caolín (kaolin) y sílice (silica), por lo que estos dos ingredientes de la receta se debe reducir para mantener la química idéntica. El carbonato de litio es refinado del mineral spodumene.

Pero, en esta receta "Degradado de Bronce Verde" "Weathered Bronze Green" el esmalte yo hecho usando spodumene ve sólo ligeramente diferente de un esmalte hecho con el mismo peso de carbonato de litio, o fluoruro de litio.

http://translate.google.com/

Lithium Carbonate, Spodumene, and Lithium Fluoride

Comment by Daniel Ramos speak-spanish. on May 17, 2015 at 6:59pm

Como se sustituye el carbonato de lithio por spedumene , es decir tengo spodumene , pero no tengo carbonato de litio , en mexico no venden litio pero si tengo spodumene ?

Comment by Cyndy Littleton on January 29, 2015 at 2:09pm

I will definitely look into those options! Thank you Juli!


Stars
Comment by juli long on January 29, 2015 at 1:30pm

I guess we could replace the barium with strontium carbonate or whiting on a  molar weight in glaze cal. and reformulate.  I'm not savvy with it though.

Comment by Cyndy Littleton on January 29, 2015 at 9:51am

The folk art guild got a lot of ooooooohhs from my clients. I like the way it breaks. I love the looks of the Buckwheat, but the barium content is a concern. If it was my studio, I would make a batch in a heartbeat.


Stars
Comment by juli long on January 29, 2015 at 9:45am

Good to see you got some tested.  i plan to do some when it warms up here. The folk art guild looks pretty promising to me (had that one in mind).

juli

Comment by Cyndy Littleton on January 28, 2015 at 6:30pm
Testing glazes from John Britt's new book

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service