Hello, I like the looks of your stuff... The Tea pot is a oribe glaze, I reduce it in a electric kiln with an addition of silican carbide in the glaze.
I am useing .7 % of Silican Carbide in my Copper Reds & Oribe glazes. I have good luck in the Oribe and starting to have good luck in my Copper Reds. In the Copper Reds I have pin holes from the Silican Carbide, but I am getting Ox Bloods. It has been a process but I am getting red. I think it will be a learning process for you, I would make a bunch of test with differing percentages of Silican Carbide, and I put a small percentage of Iron Ox. in the glaze with the Tin Ox.
Good day, I am RonaId Morris, I saw your profile and I decided to contact you immediately. Can you get back to me on my email (ronmorri01@gmail.com) for full details. Regards.
Thomas
Dec 27, 2010
Thomas
Good Morning
I am useing .7 % of Silican Carbide in my Copper Reds & Oribe glazes. I have good luck in the Oribe and starting to have good luck in my Copper Reds. In the Copper Reds I have pin holes from the Silican Carbide, but I am getting Ox Bloods. It has been a process but I am getting red. I think it will be a learning process for you, I would make a bunch of test with differing percentages of Silican Carbide, and I put a small percentage of Iron Ox. in the glaze with the Tin Ox.
Good luck...