I am at the early stages of exploring SH glazes. I have been using the base and modifiers listed on this web site as well as some details from Steve's latest DVD too. The only difference with my pieces is the layering of the different combinations and thickness of the modifiers.
I have tried to include the details as much as I can.
Hi Tom, Last time we spoke you were about to do some tests with SCM and other glazes. Just wondering how you are going with them and if you would like to share your results?
Don Olliff
Hi Tom,
Thanks for the kind words about my glazes.
I am at the early stages of exploring SH glazes. I have been using the base and modifiers listed on this web site as well as some details from Steve's latest DVD too. The only difference with my pieces is the layering of the different combinations and thickness of the modifiers.
I have tried to include the details as much as I can.
Looking forward to seeing more of your work...
Don
Mar 3, 2012
Jan Wallace
Hi Tom, Last time we spoke you were about to do some tests with SCM and other glazes. Just wondering how you are going with them and if you would like to share your results?
Apr 26, 2012
Jan Wallace
I look forward to seeing the results Tom and good luck with your teapots.