Stars

Don Olliff

Male

Deer Harbor, WA

United States

Profile Information:

What is your experience with ceramics in general. (Long answer encouraged)
About 10 years exploring clay and glazes.
What is your current involvement with electric fired ceramics? (long answer encouraged)
I have an L&L kiln and have been on a glaze mixing adventure for the last year or so.
All our content is viewable by the public. Why do you want to be a member, when you can already see everything as a non-member?
sharing knowledge
Where do you work on your ceramics projects?
home studio
How did you find this network?
referred by friend

Comment Wall:

  • Tom Waggle

    Dear Don,

    your work is beautiful and your surfaces are stunning.

    Photos 11, 12 and 15 resemble effects I have gotten in Cone 10 Soda firings with Oribe Green (turning black when sprayed thicker and the varied Matte and Gloss surface).

    Are these SH recipes or ones you have developed?

    I am just starting my journey of moving from Soda to Cone 6 Oxidation and am interested in trying to emulate my Soda work at the onset then hopefully getting to a more distinct Cone 6 surface (one that could not be obtained in Soda).

    Any help regarding this would be greatly appreciated.

    Regards,

    Tom

  • Ronald Morris

    Good day,
    I am RonaId Morris, I saw your profile and I decided to contact you immediately. Can you get back to me on my email (ronmorri01@gmail.com) for full details.
    Regards.