Started by George Lewter. Last reply by Norm Stuart Sep 29, 2017. 46 Replies 4 Likes
These are the glazes that Steven introduced us to for creating the layered effects for which he is renown. This is the place to post modifications for these glazes, and other glazes that you have found to work well with SCM and SCM for orange. …Continue
Started by Tom Waggle. Last reply by Tom Anderson Oct 17, 2016. 22 Replies 0 Likes
I sent an email out to all group members. I should have just started this thread.I am using Laguna 607 cone 6 stoneware.I am getting pinholes and craters on about 1/3 to 1/2 of my pieces.I contacted Stephen Hill via email to ask him about this. He suggested that I just switch to porcelain as it is the gasses from the impure elements in stoneware body.I have adjusted my bisque schedule to slow down to 100'/hr between 1100' and 1700' ( the temp range where those organic gasses burn off). I am…Continue
Started by Joseph Fireborn. Last reply by Norm Stuart Jul 24, 2016. 5 Replies 0 Likes
This has been created to carry over the conversation that we were having on the discussion comments instead of in a topic. I have copied and pasted the discussion that I created in order of start to current. Please lets move all topics here as it would better be searchable in the future. Comment by Joseph Fireborn I have a question about SH's pots. I have tried using SCM, I get some really nice results, but the glaze surface…Continue
Started by George Lewter Jul 12, 2016. 0 Replies 0 Likes
Numerous members have used SCM and Jen's Juicy Fruit with excellent results. I believe the crystals being objected to are some kind of crystal that is growing in the melt upon cooling, not unmelted strontium poking out of the matrix. The crystals have sharp diamond reflective points which would not be present if they had been even slightly attacked by the glaze fluxes, of which there are plenty, evidenced by the fact that the glaze is very prone to running.My understanding is that …Continue
Comment
I know of four different versions of Hannah's Fake Ash, none of which include silica - so you have a fifth recipe!
I obtained this version of Hannah's Fake Ash from the potter Yoko Sekino-Bové.
100.0% Ellen Shankin’s Fake Ash ^5 -10
60.0% Redart Clay
30.0% Whiting
10.0% Barium Carbonate
Hey guys, thanks for the comments. I thought the warm and cool versions were pretty similar, I just hoped to see if there was a discernible difference if they were both put under the same glaze. I suppose it could be different for every glaze combination.
George, I was expecting an answer like you provided. Probably too many variables for anything conclusive. It would be interesting to see how stable the glazes over SCM are compared to the glazes by themselves. I've looked at Steven Hill's site and he has a lot of great functional work but I haven't seen any mention of leach testing. Maybe I'll try to contact him and see what he has to say.
Thanks again.
Brandon, The Steven Hill portion of the download offers good examples of the SCM Warm versus Cool SCM on pages 5 (warm)and 6 (cool). He uses a warm palette SCM Warm base, and a cool palette, Cool SCM base). About 80% of a pot gets the SCM base, then 4-5 glazes are layered over. The top and bottom, or edges will typically get a contrasting glaze. Several good examples in that article.
The two are the same base, but cool is white, warm has iron added that gives it some yellow. Neither is particularly attractive alone, and are always used as base glazes, under several or many layers of other glazes with multiple heavy metal colorants.
How would you reliably leach test all the possible glaze interactions and the stability of those blends? It might give some comfort to have samples of your favorite combinations leach tested, but you still couldn't guarantee future results.
Brandon, basically the Warm SCM is a more earthy yellow/brownish color after firing. You use it with warm earthtone color schemes, ie. with yellows, browns, greens, iron saturate reds, etc. The Cool SCM is more white in color and goes better with a cooler, ice-like pallet of blue, white, grey, black type of glaze colors. If you get Steven Hill's DVD he shows examples using SCM Warm & Cool versions. I mostly work with the SCM Warm but have done a few pots with the SCM Cool.
Hello SHO Project,
Can anyone tell me (or show images) of the difference between the cool and warm versions of Strontium Crystal Magic? I downloaded a free file from Ceramic Arts Daily (free subscription required) and it listed both recipes. Link. Just curious if anyone already has some side by side comparisons. Eventually I hope to post some of my own.
Also, have there been any tests of the "food safeness" of SCM? I've seen it used on the insides of bowls but other people use a liner glaze and only have the SCM on the outside of pots. I haven't seen anyone share actual test results.
Sorry if this has already been discussed. I'm still learning to navigate the site. There is a lot of good info!
This was Posted by eleanor akowitz on December 3, 2010 at 1:59pm in Continuing Education. It got no responses there, so I'm moving it here where more people may see it, and follow the link to see the photos from the Steven Hill workshop she attended.
I highly recommend the the Steven Hill DVD to anyone who wants to learn about layering glazes, use his updated cone 6 glazes and/or firing schedules, get a feel for the man himself before doing his workshops, or as a refresher if it's been a while since you attended one of his workshops.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2025 Created by Andrea Wolf.
Powered by
You need to be a member of Steven Hill Oxidation Project to add comments!