Hello all,

I have gotten good results with the standard Steven Hill recipes (I own the DVD).
I am looking to find out if it is possible to spray a clear gloss glaze over the standard SH glazes in order to get some glossy areas?
Has anyone tried this, and if so success?
I have used a glossy white glaze as my liner glaze and along the rim of some pieces the gloss white ran down outside of my piece and created a glossy blend with the SH glazes.
I plan on doing some tests, just thought I would ask first.
Any advice or replies are much appreciated.

Views: 330

Replies to This Discussion

Water Color Green and Blue will give matte colors where thinly sprayed over SCM and the other modifier glazes. When sprayed on thicker, they will go glossy transparent and then get runny. Exercise caution.

Above is Water Color Green thin to medium over SCM. You can see it very matte but the darker areas are glossier.

The second picture is the other side of the same tankard. The band of Water Color Green is concentrated and a high gloss transparent with almost metallic reflective qualities.

Strontium Crystal Magic is a bit tricky as a base glaze. There is not a lot of latitude between being too thin and the body texture coming through, and being too thick and running off the pot. I'm guessing that it won't take much of a clear gloss cover to put most of your glaze on your kiln shelves :-(  

If what your hoping for is to look down through a clear gloss and see all that complex color and crystals that develop with these glazes, in 3-D, I'd like to see that too. Good luck!

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service