George Lewter's Discussions (470)

Discussions Replied To (35) Replies Latest Activity

"Melissa,  Strontium carbonate is much less toxic than many other ceramic materials.…"

George Lewter replied Mar 8, 2016 to The Companion Glazes - Modifiers and Complements to SCM

46 Sep 29, 2017
Reply by Norm Stuart

"Thank you, Denise. I was thinking of SH's older firing schedules from 3-4 years ago.…"

George Lewter replied Dec 14, 2014 to SCM and the Companion Glazes Run

12 Feb 2, 2015
Reply by Charna Schwartz

"Even if you are not using the Steven Hill glazes, when you are layering glazes, you…"

George Lewter replied Dec 14, 2014 to SCM and the Companion Glazes Run

12 Feb 2, 2015
Reply by Charna Schwartz

"Using 2012 updated recipes for SH Red Orange and Jen's Juicy Fruit w/ red iron oxide…"

George Lewter replied Sep 7, 2014 to The Companion Glazes - Modifiers and Complements to SCM

46 Sep 29, 2017
Reply by Norm Stuart

"Issues with Hannah's Fake Ash Blue and SH Green Ash.  My pots with HFA Blue have bee…"

George Lewter replied Nov 24, 2013 to The Companion Glazes - Modifiers and Complements to SCM

46 Sep 29, 2017
Reply by Norm Stuart

"Water Color Green and Blue will give matte colors where thinly sprayed over SCM and…"

George Lewter replied Oct 26, 2013 to Looking for glossy results with SH

1 Oct 26, 2013
Reply by George Lewter

"Lawence, you are correct that the images are a from a Filemaker application. The sof…"

George Lewter replied May 29, 2013 to The Companion Glazes - Modifiers and Complements to SCM

46 Sep 29, 2017
Reply by Norm Stuart

"What I can see is: A very nice looking set of cups. The fake ash is fully melted, w…"

George Lewter replied Apr 18, 2012 to The Companion Glazes - Modifiers and Complements to SCM

46 Sep 29, 2017
Reply by Norm Stuart

"Hm . . . You're right, June. The Hesselberth and Roy cone 6 limit formulas also set…"

George Lewter replied Apr 17, 2012 to The Companion Glazes - Modifiers and Complements to SCM

46 Sep 29, 2017
Reply by Norm Stuart

"This was under another topic: Reply by graham strong on March 23, 2012 at 8:42pmDele…"

George Lewter replied Apr 17, 2012 to The Companion Glazes - Modifiers and Complements to SCM

46 Sep 29, 2017
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service