I have noticed that glazes often tend to either react when layered or are quite stable and do not mix.  If anyone has any insights into the chemical reactions I would like hear.  It seems like there are times you would like to encourage two glazes to interact with each other.

I have heard of some artists who multifire at successively lower temperatures to allow them to layer glazes much like a painter may add colors and details successively. I have found that refiring a piece with a second glaze over the original results in little to no mixing of the glazes - usefull to change a design but why is it that the glazes don't mix?

What if you wanted to encourage this?  Would the secret be in adding flux, adding something between the two glazes?  Would it be possible to change a fired glaze after the fact by adding a layer on top and refiring (for instance I have been able to reduce crazing by refiring with a pure silica wash, crazing is reduced although the surface becomes rough and matted).

About all I know about this is zinc in a glaze can change colors in some stains and some high iron glazes can produce some nice effects as the run down the side of a pot into other color glazes.

Views: 436

Replies to This Discussion

Brent:

Flux basics- calcium, magnesium and strontium are considered low flow fluxes: meaning they have a tendency not to run. Sodium, potassium, and lithium are high flow: meaning they have a tendency to run.

The base glaze should be high in calcium, magnesium and strontium; so it will be stable. The top layer should be sodium, potassium, or lithium so that it will run.

Want more run- increase the lithium.

Want even more run: add some frit- the molten lava river.

Want to freeze the glaze in place?  add lower percentages of alumina hydrate.

Some basic principles, without paragraphs of chemistry.

Tom

rather than the flow/run what about the mixing of two glazes.  Would this imply if both are high in calcium, magnesium or strontium they won't mix and if high in sodium, potassium or lithium they would 'mix' i.e. tend towards more mixing of the colorants.

Another way to look at it is what makes one pair of glazes 'coat' one another versus what makes another pair of glazes mix and react with each other?

 

Glazes layered or in contact with each other can exhibit wild behavior due to eutectic melting. Material components that have higher melting points by themselves can have drastically reduced melting points when mixed together, or in contact with each other. Quite often two very stable glazes, individually, will run off a pot when layered together.


sounds like, experiment and test, experiment and test, experiment and test, repeat.

I am guessing the amount of soak at the target cone can have an effect as well.  so fluidity + time at temperature


George Lewter said:

Glazes layered or in contact with each other can exhibit wild behavior due to eutectic melting. Material components that have higher melting points by themselves can have drastically reduced melting points when mixed together, or in contact with each other. Quite often two very stable glazes, individually, will run off a pot when layered together.

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service