Cone 6 Glaze Testing & Reporting Discussions (14)

← Back to Cone 6 Glaze Testing & Reporting
Discussions Replies Latest Activity

Stars

Waterfall Brown with a typo.....

I'm setting up my new studio, mixing some glazes and get my first glazes unloaded. I was shocked at the Waterfall Brown as it wasn't anythi…

Started by Gina Skillings

0 Feb 23, 2018

A few hundred glaze recipes for Ye"all

I found that I had a 2013 glazechem database.There are hundreds of recipes. I extracted the recipes for you folk. The files were so large t…

Started by Lawrence Weathers

3 Jun 21, 2017
Reply by Lawrence Weathers

Stars

What causes glazes to react with each other

I have noticed that glazes often tend to either react when layered or are quite stable and do not mix.  If anyone has any insights into the…

Started by Brent Farler

4 May 18, 2017
Reply by Brent Farler

Ian Currie Grid Glaze Test Method

This is the place for all things Ian Currie Grid Test Method. Feel free to post: 1. Questions 2. Tiles you have made and interesting things…

Started by Joseph Fireborn

3 Jun 6, 2016
Reply by Joseph Fireborn

Stars

Transparent Green Glaze

Does anyone have a suggestion for a glossy, or semi-gloss, green glaze? Preferably transparent. I did locate a couple of glazes in the Insi…

Started by Dave Hodapp

11 Jun 6, 2016
Reply by June Perry

Richard Busch's Nutmeg as a base with other glazes layered over it.

I fired a bisqued Laguna #80 clay test ring consisting of a nutmeg base coat (brushed on) all the way around the ring and  9 glazes brushed…

Started by George Lewter

7 Oct 27, 2015
Reply by Randy McCall

Stars

Viscosity and surface tension

I came across a set of calculations for Viscosity and surface tension from oxide composition. Has anyone used these types of calculations t…

Started by Robert Coyle

5 Sep 16, 2015
Reply by Robert Coyle

high ball clay cone 6 glaze

 I'm fiddling with the idea of doing mocha diffusion over the top of glazes so that they come through sharper. To do this, I need a reliabl…

Started by Lawrence Weathers

0 Dec 28, 2014

MC6 Caribbean Sea Green Crawled.......

Has anyone had trouble with MC6 Caribbean Sea Green?  On my first test tile, it looked as if it vaporized.  I did not have vent on the kiln…

Started by Jane Fassel

1 Apr 15, 2014
Reply by martha peddicord

Carribean Sea

Jane- try it again- used it many times- never crawled- a beautiful glaze!

Started by phyllis schulte

0 Jan 13, 2013

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service