Thank you Norm Stuart. Save the Darvan gel-like reclaim for wheelwork!

Hi,

It has been awhile, but I have been very busy reacting to the advice given with great success, . This was exactly what I needed to do Norm. The clay restoration from slip to wheelwork experiment was done with 2x additions and I tested Bentonite Calcium 100# as well as Bentonite Calcium, "albeit at double the cost "..the. 300#.  There has been no noticeable difference between the 2 grades. I have thus decided to go with the cheaper 100# Bentonite.

For a detailed recipe and technique go to the brilliant article by: Thomas Anderson as follows.

Clay Restoration ---DIGITALFIRE.COM---

Thomas Anderson • May 6, 2019

Also a summarized method below:

SUPERCHARGE THE PLASTICITY OF CONE 6 RECLAIMED CLAY

Reclaimer contents is as follows:

50% Bentonite and 50% ball clay.

Remember to mix these 2 powders together in a plastic bag by shaking well. Bentonite is almost impossible to mix with slip or water slurry because of incredibly fine particles. This new powder will now mix readily with water to form clay on plaster with similar feel to clay that needs "repair".

These proportions fire as a tan-buff stoneware at cone 6.

Method:

Mix in 50 grams of above "reclaimer" stock, to 1kg of problem, gel-like clay to fix it for wheelwork.

Flatten both "patties" on a bat and fold both into each other 20 times to create 1 million layers! (wedging or pugging should do)

Result: Perfectly even throwing clay and incredibly plastic!

Note: The wobbly, shearing, thixotropic effect of the Darvan recycled slip is gone!!!!

Views: 185

▶ Reply to This

Replies to This Discussion

I'm glad.  You just needed to experiment until it worked right.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service