Hi
I'm trying to learn how to do mocha diffusion. I read your description along with a number of others on the web. However, I'm not having any luck getting the dendrite pattern. I will try very a lot of things and nothing seems to make much difference.

This is what I've tried:

1. Slip made of Tennessee ball clay
2. Robin Hopper's diffusion slip: (ball 75, spar 5, silica 10, epk 10) plus I add 5 3134 and 10 RIO
3. adding hardwood ash, or sodium silicate, or Calcium nitrite to the above slips

I've used thick and thin solutions of cobalt carbonate and ordinary vinegar or apple cider vinegar.

I've tried using in both horizontally and vertically on my leather hard G6 mix clay.

The very best I've done is to get some almost microscopic dendrites on the edge of my dribbles.

Also, in a CAD article Robin Hopper gives the following recipe  for diffusion slip

ball clay   75,

Feldsspar  5,

silica       10,

Kaolin      10

Does anyone know what kind of ball clay and feldspar one should use?

I would appreciate any advice or guidance you can give me in debugging this.

Thanks

Larry

 

Views: 2556

Reply to This

Replies to This Discussion

I emphasize that all discussions on special slips,  pH control and so on are just rubbish....

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service