Joan Scott's Discussions (15)

Discussions Replied To (14) Replies Latest Activity

Stars

"You could try decreasing tin and supplement with zircopax. Sometimes works in other…"

Joan Scott replied May 8, 2018 to Tin Oxide substitutes

5 May 8, 2018
Reply by Norm Stuart

"What is the colorant for seafoam as compared to bronze? I have a strong blue with 1%…"

Joan Scott replied May 2, 2018 to Pete's Weathered Bronze (Green)

17 May 2, 2018
Reply by Barbara Hanselman

Stars

"Hi George, For the model with stainless steel nozzle do you have a model number?"

Joan Scott replied Aug 15, 2016 to Spraying glazes

56 Sep 11, 2016
Reply by Jim Wallace

Stars

"Thanks Norm that is useful to know. "

Joan Scott replied May 31, 2013 to Magruder Red cone 6

29 Jun 21, 2014
Reply by Donna Kat

Stars

"Thanks for posting the tile. Is that on a stoneware tile? "

Joan Scott replied May 31, 2013 to Magruder Red cone 6

29 Jun 21, 2014
Reply by Donna Kat

Stars

"No problem, thanks. "

Joan Scott replied Apr 24, 2013 to Magruder Red cone 6

29 Jun 21, 2014
Reply by Donna Kat

Stars

"Wonderful information. Thanks. I do use neph sy frequently instead of feldspars. Can…"

Joan Scott replied Apr 24, 2013 to Magruder Red cone 6

29 Jun 21, 2014
Reply by Donna Kat

Stars

"Thanks for this. Do you have some of these slow cooling iron glazes in your photos?…"

Joan Scott replied Apr 23, 2013 to Magruder Red cone 6

29 Jun 21, 2014
Reply by Donna Kat

Stars

"Tin is very expensive to use but I have found that in some particular glazes and esp…"

Joan Scott replied Apr 23, 2013 to Magruder Red cone 6

29 Jun 21, 2014
Reply by Donna Kat

Stars

"Interesting information. I have this for ORANGE STREET:Silica 15.2%Talc 13.8%Dolomit…"

Joan Scott replied Apr 23, 2013 to Magruder Red cone 6

29 Jun 21, 2014
Reply by Donna Kat

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service