Wyndham Dennison's Discussions (15)

Discussions Replied To (14) Replies Latest Activity

Stars

"just a arbitrary number that seems to work in most glazes. More than 10% raw clay se…"

Wyndham Dennison replied Sep 5, 2017 to Silky Matte - Digitalfire - Tony Hansen

9 Sep 5, 2017
Reply by Wyndham Dennison

Stars

"Norm, I like your test. Have a question on the amt of epk used vs calcined glomax. I…"

Wyndham Dennison replied Sep 5, 2017 to Silky Matte - Digitalfire - Tony Hansen

9 Sep 5, 2017
Reply by Wyndham Dennison

"Tony Hanson at digitalfire has a discussion on rutile blues and slip clays, a good r…"

Wyndham Dennison replied Jan 11, 2017 to Light Rutile Substitute

11 Mar 7, 2017
Reply by Judith Stoudmann

"You know rutile is used  as a flux compound in welding. If I remember you can buy ru…"

Wyndham Dennison replied Jan 11, 2017 to Light Rutile Substitute

11 Mar 7, 2017
Reply by Judith Stoudmann

"I use titanium at 93% and RIO 7%, which for my glazes work fine, if it's too dark b…"

Wyndham Dennison replied Jan 9, 2017 to Light Rutile Substitute

11 Mar 7, 2017
Reply by Judith Stoudmann

"There are several silky/satin whites that fire to cone 10. Leach white is one of the…"

Wyndham Dennison replied Jul 14, 2014 to Looking for creamy white glaze for red clay

5 Oct 4, 2014
Reply by Harold Roberts

"Thanks,Oh I will definitely do some line test, but thought someone here might know a…"

Wyndham Dennison replied Jul 13, 2014 to opulence matt base question

3 Jul 13, 2014
Reply by Wyndham Dennison

"There's another possible way to help trap the copper Make glaze "A"(goes on first) w…"

Wyndham Dennison replied Jul 5, 2014 to silicon carbide in red reduction glazes for an oxidation environment?

12 Jul 7, 2014
Reply by Jeff Poulter

Stars

"The other point I wanted to share is that the mass of the kiln at 2232 might be comp…"

Wyndham Dennison replied May 23, 2014 to Slow Cooling

13 Jun 28, 2017
Reply by Norm Stuart

Stars

"I agree about the crystallization range. When I fire my crystalline glazes to cone 1…"

Wyndham Dennison replied May 23, 2014 to Slow Cooling

13 Jun 28, 2017
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service