I have set up a web site with glaze tests for any one interested.  Tried an true recipes that are some of my favorites.

mccallsc.tripod.com

Site is better with Opera or Chrome

Views: 4434

▶ Reply to This

Replies to This Discussion

interestin, I have used Ellen Buff for years with no problems, then this summer, zit city.  Called Highwater, they said I should come take their claze class !! All my other clays do fine, and I love Redstone, both for throwability and glaze color.

But I do want a buff clay.  Waynesboro, from Bryan Fort in Ga, is nice.

I'm interested in the comment you made on you glaze testing site, very nice , by the way.  You reccommend holding bisque for 5 hours at medium temp.  What do you mean, hold at What temp, and for 5 hours ? long time.  I have a computer controll Skutt 1027, and bisque fire to ^04, what Highwater recommends. 

Randy, I really liked your glaze testing and I was going to try your glaze "nutmeg variation", but i have a question before I order the spodumene-gwalia. Can I substitute plain spodumene, or does it need

to be "Gwalia"? Is there a big difference? Hope to hear from you soon.

Juli

Randy, 

I checked with my supplier, and after some research they concluded their spodumene was Gwilia.

I'm good to go. Trinity ceramics in Dallas, supplier .

juli

juli long said:

Randy, I really liked your glaze testing and I was going to try your glaze "nutmeg variation", but i have a question before I order the spodumene-gwalia. Can I substitute plain spodumene, or does it need

to be "Gwalia"? Is there a big difference? Hope to hear from you soon.

Juli

Juli - According to Digitalfire, Australian spodumene is considered the whitest burning spodumene in the world.

http://digitalfire.com/4sight/material/australian_spodumene_2275.html

Old recipes typically call for spodumene concentrate, either Gwalia Australian or Foote from North Carolina - neither name currently exists.

The Foote mine was exhausted some years ago and the Sons of Gwalia mining company, founded and originally managed by pre-President Herbert Hoover, became insolvent in 2004 and is no more.  Talison currently mines the Gwalia Greenbushes spodumene mine and sells it through a number of distributors who use different marketing names.

Digitalfire has five or so different analyses for spodumene concentrates. You could compare your spodume analysis with the Australian spodumene above. Our 20 year old bag of Gwalia is half-full, so I'll face the same sourcing problem when it's empty.

If your bag is from the old Gwalia mine, it could be labelled Talison, or Chengdu Tianqi the Chinese company which is currently acquiring Talison and their former Gwalia Greenbushes mine.

The Talison Brand

http://www.ccnmatthews.com/logos/20110413-TALI.gif


Thanks Norm for all the info!  I just hope it makes my glaze fabulous. Its a tricky word to pronounce.

Juli

Norm Stuart said:

Juli - According to Digitalfire, Australian spodumene is considered the whitest burning spodumene in the world.

http://digitalfire.com/4sight/material/australian_spodumene_2275.html

Old recipes typically call for spodumene concentrate, either Gwalia Australian or Foote from North Carolina - neither name currently exists.

The Foote mine was exhausted some years ago and the Sons of Gwalia mining company, founded and originally managed by pre-President Herbert Hoover, became insolvent in 2004 and is no more.  Talison currently mines the Gwalia Greenbushes spodumene mine and sells it through a number of distributors who use different marketing names.

Digitalfire has five or so different analyses for spodumene concentrates. You could compare your spodume analysis with the Australian spodumene above. Our 20 year old bag of Gwalia is half-full, so I'll face the same sourcing problem when it's empty.

If your bag is from the old Gwalia mine, it could be labelled Talison, or Chengdu Tianqi the Chinese company which is currently acquiring Talison and their former Gwalia Greenbushes mine.

The Talison Brand

http://www.ccnmatthews.com/logos/20110413-TALI.gif

Great. I will try your glazes

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service