George Lewter's Discussions (470)

Discussions Replied To (229) Replies Latest Activity

"I'm not sure what you gain by spraying (underglaze?) on greenware, rather than waiti…"

George Lewter replied Jul 20, 2014 to Single fire a sculpture?

4 Jul 24, 2014
Reply by George Lewter

"If you have a kiln sitter keep firing until it trips as it measures heat work. If no…"

George Lewter replied Jun 11, 2014 to Firing too long at lower cone a problem?

7 Jun 21, 2014
Reply by Meredith Walker

"Skimlinks scans our entire site and turns mention of products into shopping links th…"

George Lewter replied May 10, 2014 to Supporting Links

9 May 20, 2014
Reply by Nadine Mercader

"Daniel, what is the long diagonal swath from lower left to middle right?"

George Lewter replied May 10, 2014 to Can one predict the appearance of a glaze? (part I: The Si/Al ratio)

9 Oct 19, 2016
Reply by Tom Humphries

"Thanks, Nadine I will be writing up details about how we get commissions on sales th…"

George Lewter replied May 10, 2014 to Supporting Links

9 May 20, 2014
Reply by Nadine Mercader

"Any member can add inline pictures to their discussion or blog postings. See the Pic…"

George Lewter replied May 9, 2014 to White suger powder lookalike glaze

4 May 9, 2014
Reply by George Lewter

"I put the image directly into your posting so people don't have to open it to see."

George Lewter replied May 9, 2014 to White suger powder lookalike glaze

4 May 9, 2014
Reply by George Lewter

"Interesting effect. Like snow fall. I would test the whitest clay I can find and try…"

George Lewter replied May 9, 2014 to White suger powder lookalike glaze

4 May 9, 2014
Reply by George Lewter

"Troy Bungart makes paint brushes. Talk to him."

George Lewter replied May 1, 2014 to Chinese Brush Painting

1 May 1, 2014
Reply by George Lewter

"The soak at the top of any firing curve is to give the glaze a chance to develop --…"

George Lewter replied Apr 24, 2014 to Stephen Hill firing schedule

4 Apr 25, 2014
Reply by Lawrence Weathers

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service