Norm Stuart's Discussions (511)

Discussions Replied To (426) Replies Latest Activity

"I can't think of a reason you can't reduce the amount of kaolin to 10% by replacing…"

Norm Stuart replied Sep 5, 2017 to Silky Matte - Digitalfire - Tony Hansen

9 Sep 5, 2017
Reply by Wyndham Dennison

"Yes. unless you can create a magic frictionless surface either the metal will wear-o…"

Norm Stuart replied Aug 23, 2017 to Silky Matte - Digitalfire - Tony Hansen

9 Sep 5, 2017
Reply by Wyndham Dennison

"Tony Hansen's new Silky Matte is much harder than cutlery. So I can easily make cutl…"

Norm Stuart replied Aug 23, 2017 to Silky Matte - Digitalfire - Tony Hansen

9 Sep 5, 2017
Reply by Wyndham Dennison

"The two "Chemically Identical Glazes" fired exactly the same in spite of different i…"

Norm Stuart replied Aug 18, 2017 to Silky Matte - Digitalfire - Tony Hansen

9 Sep 5, 2017
Reply by Wyndham Dennison

"Our electrician double-jacked the main before the breaker-box, live to install our b…"

Norm Stuart replied Aug 2, 2017 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"You can add the amp sensor to the older V6-CF Bartlett as well. The amperage test is…"

Norm Stuart replied Jul 31, 2017 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"Genesis Controller installed with extra aluminum plate to cover hole from original k…"

Norm Stuart replied Jul 28, 2017 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"Carl - We used a lot of WC‑436 B‑Mix 5 Clay with Grog from our last order. Nice text…"

Norm Stuart replied Jul 26, 2017 to Looking for a clay

1 Jul 26, 2017
Reply by Norm Stuart

"Someone will need to volunteer a Dropbox or other website to host the files and I'll…"

Norm Stuart replied Jul 15, 2017 to Alfred University Fundamentals of Ceramics

13 May 3, 2021
Reply by cp dunbar

"Crocus Martis has two explanations. The first explanation was it was a natural hydra…"

Norm Stuart replied Jul 1, 2017 to Penland Red-Orange posted by Michele Hartung 6/29/2011

17 Jul 1, 2017
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service