Jeff Poulter's Discussions (111)

Discussions Replied To (98) Replies Latest Activity

Stars

"I had to do some digging, but I found the pics.  These were junker fruit bowls that…"

Jeff Poulter replied Feb 25, 2014 to Refire Test Ring from previous Cone 6 Test to 1000c and Intereting Results

9 Feb 25, 2014
Reply by Norm Stuart

"You could always use a black stoneware.  They are usually not cheap & they will…"

Jeff Poulter replied Feb 25, 2014 to From raku to stoneware

4 Mar 27, 2014
Reply by Jennifer Arthur

Stars

"I thought I had posted pictures for this. I'll have to wait until I get to work and…"

Jeff Poulter replied Feb 15, 2014 to Refire Test Ring from previous Cone 6 Test to 1000c and Intereting Results

9 Feb 25, 2014
Reply by Norm Stuart

"Thanks Tracy!  Bear in mind that I have not taken these to ^10, but only to ^5.  The…"

Jeff Poulter replied Jan 5, 2014 to Fused Ornaments

4 Jan 5, 2014
Reply by Jeff Poulter

"The rods are from Kemper & are CBBH bars.  They are 11" long & $6.45/each fo…"

Jeff Poulter replied Jan 5, 2014 to Fused Ornaments

4 Jan 5, 2014
Reply by Jeff Poulter

"I bought some heavy duty rods, cut them in half & stuck them in a soft brick. I…"

Jeff Poulter replied Jan 5, 2014 to Fused Ornaments

4 Jan 5, 2014
Reply by Jeff Poulter

"You can get some plug & play controllers off of e-bay for less than $500.00.  Yo…"

Jeff Poulter replied Nov 11, 2013 to hold cycle

11 Nov 13, 2013
Reply by Norm Stuart

"I thought that someone replied on Peter's blog about converting these glazes to ^6.…"

Jeff Poulter replied Oct 1, 2013 to Chun (jun) glazes

5 Oct 4, 2013
Reply by Jennifer Arthur

Stars

"OK, I lied! I have user 1 on my e18t programmed to do a 9999 ramp to 100c for when I…"

Jeff Poulter replied Aug 26, 2013 to Kiln Element Life

18 Mar 10, 2015
Reply by Jeff Poulter

Stars

"My L&L e18t only pulls 35 amps to produce 8400 watts, but it is only 18"wide &am…"

Jeff Poulter replied Aug 26, 2013 to Firing Schedule - Fine tuning your electric kiln controller

45 Aug 27, 2013
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service