Norm Stuart's Discussions (511)

Discussions Replied To (426) Replies Latest Activity

"The purpose of a short hold, on the order of ten minutes, is to equalize the tempera…"

Norm Stuart replied Oct 25, 2013 to hold cycle

11 Nov 13, 2013
Reply by Norm Stuart

"Using G-200HP feldspar, instead of Custer, replaces 2.1% Na flux with K flux, and in…"

Norm Stuart replied Oct 20, 2013 to How Can I Substitute G200 hp for Custer Feldspar

4 Mar 11, 2014
Reply by George Lewter

"Importing Laguna's Gerstley Borate from Laguna Clay, the company which now owns the…"

Norm Stuart replied Oct 9, 2013 to Gerstley borate

6 Jan 10, 2014
Reply by Jennifer Arthur

"There are a number of ^6 glazes which "over-crystallize" at a very slow-cool, leavin…"

Norm Stuart replied Oct 6, 2013 to Is C Harris Temoku a stable Iron Red Recipe for Cone 6

19 Dec 12, 2018
Reply by Norm Stuart

"Below cone 6 temperatures using a pure synthetic red iron oxide is similar to using…"

Norm Stuart replied Oct 6, 2013 to Is C Harris Temoku a stable Iron Red Recipe for Cone 6

19 Dec 12, 2018
Reply by Norm Stuart

"Eu estava visitando Lisboa e na última semana Algarve. É muito bonito, mas pode não…"

Norm Stuart replied Sep 26, 2013 to Urgent - Please Help Me - I'm Starting

2 Sep 27, 2013
Reply by Maria Correia

"Recipe calls for: 10.0 grams Copper Oxide           use 13.9 grams Copper Carbonate…"

Norm Stuart replied Sep 2, 2013 to Cobalt Oxide versu Cobalt Carbonnate

4 Sep 2, 2013
Reply by Norm Stuart

"Our studio is in a retail area and I think the veterinary hospital next door switche…"

Norm Stuart replied Aug 27, 2013 to Firing Schedule - Fine tuning your electric kiln controller

45 Aug 27, 2013
Reply by Norm Stuart

"If hard wiring is dissuasive, that's often accompanied by the use of three phase AC,…"

Norm Stuart replied Aug 27, 2013 to Firing Schedule - Fine tuning your electric kiln controller

45 Aug 27, 2013
Reply by Norm Stuart

"Now you tell me, after I had to see how fast our new kiln was at 9999 ramp. "

Norm Stuart replied Aug 26, 2013 to Kiln Element Life

18 Mar 10, 2015
Reply by Jeff Poulter

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service