Norm Stuart's Discussions (511)

Discussions Replied To (426) Replies Latest Activity

"Solid State Relays work the same way mechanical relays do. The control system, a mic…"

Norm Stuart replied Mar 10, 2015 to Kiln Element Life

18 Mar 10, 2015
Reply by Jeff Poulter

"This is a good place to compare prices on the brands you're looking at. http://www.c…"

Norm Stuart replied Mar 9, 2015 to Kiln Comparisons

7 Mar 10, 2015
Reply by Gina Skillings

"If your kiln controller can be reset for a platinum thermocouple, we have found that…"

Norm Stuart replied Mar 9, 2015 to Kiln Element Life

18 Mar 10, 2015
Reply by Jeff Poulter

"It would be very interesting to compare a small batch of Orange Street with the Synt…"

Norm Stuart replied Mar 9, 2015 to Crocus Martis

4 Mar 9, 2015
Reply by Kim Estares

"Orange Street is one of my favorite glazes.  I use a nice synthetic red iron oxide a…"

Norm Stuart replied Mar 7, 2015 to Crocus Martis

4 Mar 9, 2015
Reply by Kim Estares

"Yes - if you use water from a "water softener" it will lead to glazes settling out.…"

Norm Stuart replied Feb 18, 2015 to Water to mix glaze

3 Feb 19, 2015
Reply by Margaret Edington

"This plate was the "Mastering Cone 6 Glazes" ^6 Majolica, but made with 10% Tin Diox…"

Norm Stuart replied Feb 17, 2015 to Colorants for Glaze and Clay

4 Feb 17, 2015
Reply by Norm Stuart

"I've been very impressed with white-burning Bentone EW from China, available from Tr…"

Norm Stuart replied Feb 11, 2015 to Gerstley Borate in the USA

2 Jul 25, 2016
Reply by Tom Anderson

"I'm delighted you like the Glaze Spreadsheet.  If you have any questions just ask.…"

Norm Stuart replied Feb 4, 2015 to Glaze Calculation Software - Pro's / Con's - Which Program

17 Mar 11, 2015
Reply by Gina Skillings

"A ceramic "mocha diffusion" is merely a ceramic colorant mixed with an acid. The aci…"

Norm Stuart replied Feb 1, 2015 to Mocha diffusion tobacco tea

2 Feb 1, 2015
Reply by George Lewter

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service