Hi all, 

I'm new to cone 6 and have moved studio to town. 

I'm wondering if the town water is messing with the glaze. It seems to be precipitating out and forming thick sludge at the bottom. I have a water softener. Should I be using distilled water to mix glaze?

My previous studio had a dug well.

Views: 343

Reply to This

Replies to This Discussion

Hi Margaret,

Hope you ski day was good - I moved from Toronto to Fergus and like you I now have a water softener.

I have not experience any additional difficulty with my glazes.

Does you recipe include 'bentonite'?    Bentonite in glazes helps keep molecules in suspension.  Try to add 2 to 3 % to your recipe.   Which glaze are you using?

Denise

Yes - if you use water from a "water softener" it will lead to glazes settling out.

Two basic concepts:


1.) To help suspend glazes, I add Calcium Chloride (Ca2+) while others add Magnesium Sulphate (Mg2+) (epsom salts).

2.) If you add a feldspar high in sodium, like Nepheline Syenite, over time bacterial action can cause sodium ions (Na+) to leech into the glaze leading it to hard pan, requiring the addition of more Calcium or Magnesium ions.

Water with lots of Calcium and Magnesium ions is the definition of hard water, which helps suspend clay-like material.

A "Water Softener" has resins which attract Calcium and Magnesium ions (see #1 above) and replaces them with Sodium ions (see #2 above). When it comes time to recharge, you soak the resins with a very concentrated solution of sodium chloride salt which once again displaces the Calcium and Magnesium ions from the resin with Sodium ions. The Calcium and Magnesium ions are flushed down the drain along with the excess salt.

By definition, a "water softener" takes water which helps clay-like materials and glazes suspend, and changes it into water which tends to make clay suspensions collapse.

You either need to use water before it is "softened", or you need to add Calcium Chloride (ice-melting crystals) or Magnesium Sulphate (epsom salts). In my experience Calcium  Chloride will make fewer visual changes to the fired glaze. Calcium Chloride attracts moisture from the air, dissolving the crystals, so keep it sealed if you like the convenience of adding crystals.

http://www.amazon.com/Snow-Joe-MELT25CC-Chloride-Resealable/dp/B00O...

Occasionally glaze recipes have less than 10% clay or kaolin which will need the addition of Bentone-EW or other highly ionic bentonite / macloid product to create enough suspension. Without enough clay-like material there is nothing for the Calcium or Magnesium ions to repel. But without the positive Calcium or Magnesium ions, not even a glaze recipe with a lot of clay will remain suspended for long.

Thank you both very much for your answers. I will try these suggestions. In the meantime I have been using distilled water.

Margaret



Denise Rainville said:

Hi Margaret,

Hope you ski day was good - I moved from Toronto to Fergus and like you I now have a water softener.

I have not experience any additional difficulty with my glazes.

Does you recipe include 'bentonite'?    Bentonite in glazes helps keep molecules in suspension.  Try to add 2 to 3 % to your recipe.   Which glaze are you using?

Denise

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service