Norm Stuart's Discussions (511)

Discussions Replied To (426) Replies Latest Activity

"If you install solid state relays, in the hidden menu you can choose a CYCL time of…"

Norm Stuart replied Dec 18, 2015 to Home grown Kiln controller

12 Jan 13, 2016
Reply by Marina Reijsmeijer (Kleierij)

"Robert - The programmed fire needs to calculate and update a desired target temperat…"

Norm Stuart replied Dec 17, 2015 to Home grown Kiln controller

12 Jan 13, 2016
Reply by Marina Reijsmeijer (Kleierij)

"Weathered Bronze Green normally settles badly due to being 60% nepheline syenite, 20…"

Norm Stuart replied Dec 7, 2015 to Flocculating and deflocculating

22 Jun 17, 2019
Reply by Sharon Canfield

"Ammonium Sulfate appears to be an ideal flocculant to keep glazes suspended. It's w…"

Norm Stuart replied Nov 15, 2015 to Flocculating and deflocculating

22 Jun 17, 2019
Reply by Sharon Canfield

"If you add a glaze flocculant and it doesn't work as expected, there's likely a reas…"

Norm Stuart replied Nov 11, 2015 to Flocculating and deflocculating

22 Jun 17, 2019
Reply by Sharon Canfield

"I honestly don't understand the "assured fit" concept of firing things with lids. If…"

Norm Stuart replied Nov 4, 2015 to Firing pots with lids on

3 Nov 4, 2015
Reply by Norm Stuart

"I've read most Cone 6 glazes supposedly start to "set-up" at 1,800 F, and are nearl…"

Norm Stuart replied Nov 3, 2015 to Flocculating and deflocculating

22 Jun 17, 2019
Reply by Sharon Canfield

"Tom - I do not bisque-fire or glaze-fire jars with the lids on.   1.) The lid traps…"

Norm Stuart replied Nov 3, 2015 to Firing pots with lids on

3 Nov 4, 2015
Reply by Norm Stuart

"I think it's easiest to focus on Calcium Ca+2 and Magnesium Mg+2 ions, which floccul…"

Norm Stuart replied Nov 3, 2015 to Flocculating and deflocculating

22 Jun 17, 2019
Reply by Sharon Canfield

"Brenda - If you don't yet have a membership to Digitalfire I highly recommend it. -…"

Norm Stuart replied Oct 27, 2015 to Inquiry: Intermediate or advanced students WEEK-LONG or longer

3 Oct 27, 2015
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service