I have set up a web site with glaze tests for any one interested.  Tried an true recipes that are some of my favorites.

mccallsc.tripod.com

Site is better with Opera or Chrome

Views: 4431

▶ Reply to This

Replies to This Discussion

Leach clear. I usually brush on one coat and spoung one one coat. Don't get it thick or it will get milky. One pour on coat not too thick would probably work too. Experiment.

Thanks. I've been really leary of "clear" glazes.  I make monster mugs and on a couple of them, their eyes wound up looking like they have cataracts. I've been very careful since then. I make the clear glaze THIN -- more like milk than heavy cream. I usually brush on ONE coat. 

But like you said -- experiment!!!

Here's my facebook Monstermugs page. 
https://www.facebook.com/pages/MonsterMugs/154842774541834?sk=wall

Randy I've just mixed up some Rowe's Brown.  Does this glaze run? I'm going to put it on a cookie, just in case, but I'd like to hear from you since you are experienced with it. 

I really really appreciate these glaze recipes you've posted at the link above. 

I'll post pics of my results.

 Thanks again!

DJ

No it does not run.  Hope you can use the glazes.  These are some of the most reliable

glazes I have come across in my thirty years of pottery.  They are especially useful in layering and that

is where it is at a Cone 6.  They are all public glazes as far as I know.  just sharing like so many have done for me.....

thanks again for posting them. I intend to have a lot of fun mixing them and using them!!

I just mixed up the C Harris Tenmoku.  It called for Ball Clay #1 -- but all I had was either Tennessee ball clay or OM-4. So I used the Tennessee ball clay.  I'll post pics of how it came out.  Where does one get Ball Clay #1? Our ceramic store is rather limited in its ball clays.

The version listed by George in the database here uses EPK.. Maybe George can pipe in here.  jhp

Either will work,  The main thing with this glase is to use special rio.  This is the pure form.

What special rio? I just used regular Red Iron Oxide. 

Site seems to be working ok now in Explorer 8 you just have to scroll down to get past
advertizements.

just curious, I'm having some pinholing. what clay did you change from and to what?

I was using ellen buff from highwater and changed to red stone no more pinholes.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service