Is there anyone who uses the ash produced by pellet stoves and has experience on its use?
I'm wondering if there are any problems using this ash: I got the impression that the ash is coarser than the fireplace ash.
Actually the real difference is perhaps that the ash from the pellet stove is fine and fairly homogeneous but has few very thin particles: it seems fine, because there are not big pieces of coal but perhaps the really thin particles are missing because of the forced stove ventilation. Once washed, the ash from the pellet stove is more difficult to filter and remains darker, sometimes almost black. 

Is it possible that this aspect gives problems? Can it be solved in your opinion with some adjustments on the stove?

First photo is wood ash from fireplace

Second photo is from pellet stove

The red and blue effect in the photos is a camera fault.

Views: 238

▶ Reply to This

Replies to This Discussion

Washing the Ash

There are two differing views on whether or not ash should be washed. When it’s washed, various soluble alkaline materials are removed in solution with the washing water, and many feel that they’re throwing away precious trace ingredients and fluxes. The reasons for removing these materials are that they might enter the pores of the clay body and create various problems when they melt, and that they’re caustic. However, this is a personal choice generally best made from the experience of doing it both ways. Personally, I prefer to use unwashed ash with the soluble materials intact.

https://ceramicartsnetwork.org/pottery-making-illustrated/ceramic-s...

Thank you Norm Stuart for your replay,

at the moment I prefer to use washed ash for some different reason: one is that it is less dangerous and give me less problems with glazes, the second is that I'm trying to use as a substitute of whiting.

I'm firing between cone 6 and cone 7.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service