I must admit, I've never been terribly disciplined about my test tiles through the years.  I'm pretty good about taking careful notes; too many times I've been burned by shoddy notes.  However, I do tend to slap those careful tests on whatever's laying around.  The result is a box full of well-documented, mismatched shapes and shards.





I finally got sick of the mess.  It prompted me to search for a standardized test tile.  Many options were considered: wheel-thrown, slab-built, pinched, and free-formed.  Eventually, I settled on an extruded tube, a variation on something I saw Bill Van Guilder using.  

These tubes are uniform, stable, strong, and provide for a lot of information in a relatively small space.  They look great in a box or hanging on the wall, and they feel good to the touch.  That's my favorite part.  About the only thing they don't do is replicate a thrown surface.  I figure I can live without that.  After nine months of using them, I can tell you the time and effort it takes to produce these things ahead of time is well worth it.  It reminds me: if something is worth doing, it's worth doing it right.  ∆

Views: 369

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Norm Stuart on September 14, 2016 at 8:40pm

As you can see in Insight-Live most of our test tiles are made of scraps from my husband hand-building.

I've always liked to have the glaze showing the bottom 1/3 with one-dip, two-dips in the middle and three-dips on the top so people can see variation and especially how much the glaze runs  - pretty obvious if the demarcation between dips is not obvious.

I write on the bottom with iron oxide mixed with propylene glycol, which is wiped-out if a glaze runs too much.

When I've extruded tube test-tiles before, as I cut each segment off I smack it end-down on the table so that end has enough flat surface area to provide a stable base.

But in the end, photos of test tiles last far longer than the test tiles themselves. I just takes someone to drop it and there's roughly a 50% chance it's in pieces.

I've been having fun adding 5% alumina hydrate to glazes which run, typically bringing the Silica to Alumina ratio down to 4:1 ending up with the same glaze, slightly more matte but definitely better behaved not moving past where I place it.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service