Last year we searched for "Glaze Crystals" for a granite look or other crystal glazes and found the industry supplier in Maryland.  They melt into larger patterns at ^6, pictured below at ^06.

Tangerine glaze crystals in a yellow mason stain glaze are shown below inside a "Chippendale furniture" looking piece I made using porcelain over paper-clay so the porcelain cracks.

http://www.rabcospecks.com/home.cfm

FLG-541 Red Crystals 6/16 Mesh

To use their "online store" you need to request a catalog.  We ordered mostly larger mesh and crush them if people want smaller crystals.  You can combine them to make any of the looks shown in these prepared Mayco Jungle Gem glazes.

http://www.maycocolors.com/index.php?option=com_virtuemart&cate...

The price per pound we paid, comparable to Mason Colors - they have many other colors to choose from:

$13.85  _ FLG-460  _ Dark Golden Rod Crystals 6/16/Mesh (8 oz)
$14.08  _ FLG-470  _ White Crystals 6/10 Mesh  (8 oz)
$14.68  _ FLG-489  _ Moss Green Crystals 6/20 Mesh (8 oz)
$14.08  _ FLG-491  _ Chartreuse Crystals 6/20 Mesh  (8 oz)
$16.73  _ FLG-495  _ Yellow Crystals 6/20 Mesh (8 oz)
$15.28  _ FLG-514  _ Burnt Orange Crystals 6/20 Mesh (8 oz)
$19.38  _ FLG-541  _ Red Crystals 6/16 Mesh (8 oz)
$15.05  _ FLG-547  _ Blue Crystals 6/20 Mesh (8 oz)
$14.85  _ FLG-555  _ Tangerine Crystals 6/20 Mesh
$14.08

 _ FLG-556  _ Reactive Metallic Crystals 6/16 Mesh (8 oz)

Views: 147

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service