Check this out- same glaze, different cooling cycle- Red from MC6 Waterfall Brown

I have been trying to get iron red out of my kiln ever since I replaced it. Kept trying to slow cool from 1800 F down to 1500 F- This is proving to me that the "sweet spot" is lower in temp than I've been going. In an attempt to save a load of tableware through its slow cool cycle after my sitter tripped and stopped the kiln, I ramped it back up from 1227 up to 1800 and then slow cooled, 150 per hour to 1500. Somewhere in the process I turned all of my brown dishes red/orange. After putting them back in the kiln and refiring to cone 6, they darkened up to a much nicer red, with dark flecks and fun stuff on the surface. They don't match the rest of the set, but they are kind of cool.

The saga continues.

8/18 update(and note to self): 1250 degrees is not hot enough. I did a low bisque of pots (^018 with a 15 min hold) with terra sig on them for a barrel firing and threw in some wfl brown test pots to see if they'd turn. No dice. Next test will be closer to 1500, I guess.

Latest- magic temp for me is 1650 F with an hour hold- I then slow cool, 150 per hr, to 1400.

Views: 1553

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Tracy Shea on October 29, 2012 at 8:04pm

That is right, Brent. It works that way, too.

 

Comment by Brent Farler on October 29, 2012 at 7:19pm

I think if you put one of your waterfall brown pieces in with a bisque fire you will get the same result.  the secret is getting enough time at the temperature range where the red iron crystal grow, which is supposed to be in the 1730 degree range.

Comment by Tracy Shea on November 13, 2010 at 12:38pm
nothing magical...450 degrees per hour up to 2000F, 200 up to 2174F, 250 down to 1650, hold for 1 hour, off.
Comment by Mary Jane on November 8, 2010 at 7:06pm
Hi Tracy - The pictures are terrific. You mentioned that the magic temperature was 1650 for a 1 hour hold on the way down. I just wanted to verify the rest of the firing program. I have recently been doing cone 10 reduction firing, but want to start doing more cone 6 firings. The information here is really wonderful. Thx in advance.
Comment by Tracy Shea on November 8, 2010 at 10:47am
I started with an old, 10 cu. ft Skutt kiln. Once ^6 witness cone started going over, I turned it from high to medium for 2 hours, then off. It worked. I got an analog pyrometer to track my results. Once I got my computer controlled kiln, I lost my red. I thought it was the cool, and not a temp hold, that did it. So, I never kept track of the lower temp hold and had to start from scratch.
Comment by Tracy Shea on November 8, 2010 at 8:14am
yes, ^6, oxidation- sorry, should have indicated that.
Comment by Tracy Shea on September 14, 2010 at 11:57am
FOUND IT!! the magic temp in my kiln is 1650 for 1 hour.
Comment by Tracy Shea on August 18, 2010 at 4:19am
It's Standard 211 "hazelnut brown" clay- sorry for the delayed answer, I had not seen your comment until now :)
Comment by Mary Jane on July 20, 2010 at 12:06pm
Hi -what is the claybody that you are using? Thx, MJ
Comment by Kitoi on May 2, 2010 at 7:44pm
Haven't tried ramping it up, will have to give it a try. I've tried various cooling schedules getting nice browns but never coming close to red.

Thanks for the insight.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service