Check out the new Coyote glazes. 3 macros, an Aventurine & an Iron Red. All slow-cooled......jhp
Comment
Jeff - It's nice that commercial glaze makers have begun to sell macro-crystalline and slow-cool products.
I proves macro-crystalline glazes don't inherently have to run all over the place. The blue is nice.
So here are the 3 macros. They are very well behaved. My Skutt errored out and I Had to respray them with more glaze & fire them in my L&L. They wouldn't have run at all had I just fired them in my L&L first. I did not cool all the way to 1400F as suggested, but stopped at 1700F, then ramped back up to 1850, held, & then went 50F/hr down to 1650, held & then off. I like the Lagoon on the best..... jhp
Hi Nadine,
As soon as they get here & I have a chance to try them out, I will let you know. I'm with Norm on this. It can be done. My friend has done it & there are several several others out there that have done it. Now Coyote. It's all in the formulation. I've been chasing it for a long time. jhp
Macro-crystalline glazes require a large amount of zinc and silica to form zinc silicate crystals, and thus a fairly high ratio of silica to alumina.
But in my experience this doesn't mean macro-crystalline glazes have to be formulated in a way they're so fluid they require glaze catchers. I think those are merely the most commonly used formulations.
I too would like to hear users feedback as to the flow rates of these slow-cool Coyote glazes, but the glaze and the firing could easily be formulated to minimize flow.
Most published macro-crystalline firing techniques call have the kiln linger far longer at higher temperatures, often with repeated cycles - leading to large quantities of glaze flow.
Coyote is calling for a relatively fast slow-cool of 125 F per hour between 2,150 and 1,400 F - a wider temperature range of slow-cooling than the 1,800 to 1,500 F range we use at 50 F per hour.
Crystal Lagoon

Mars Red Iron

Ivory Crystal

Crystal Celadon

Autumn Spice

The hyperlink is below.....
coyoteclay.com

Heres one, I can't get the rest to work jhp
Jeff - photos or links?
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2025 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics