Potters & Sculptors - Making Rock from Mud
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2026 Created by Andrea Wolf.
Powered by
Comment Wall (5 comments)
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics
Good day,
I am Ronald Morris, I saw your profile and I decided to contact you immediately. Can you get back to me on my email (ronmorri01@gmail.com) for full details.
Regards.
I called Amaco to see if LUGs produced same effects as Velvets in this lowfire combo as well as at cone 5.I have not heard back. They show the Velvets at cone 5 and 10 but not LUGs. I am hoping they do as they are significantly less expensive in pint jars. I would like to be able to use them in several applications, low and cone six. I will pass on if I hear they perform as well as Velvets at Mid and High. Or if they don't.
Katherine
I miss the coast, I grew up in that area and am land locked in Ohio.
Have a great weekend.
Katherine
Have you tried Thermofax? I am trying to decide whether to invest in that, typical screens and emulsions, or maybe using EZ Screens that require no emulsions ect. I got the chance to attend one of Jason Burnette's workshops recently. He is featured in Sept/Oct Pottery Making Illustrated and he uses traditional screen printing on newsprint.
I am trying to figure what the easiest, most economical and versatile method is right for me. If you have any suggestions on which direction to pursue they would be greatly appreciated.
Katherine
StarsPatricia Sadler Trainor said…