Finally getting iron red to show up as red instead of mud

Views: 232

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Catherine Rehbein on May 15, 2011 at 7:20am
Sorry George I failed to see your statement below ....this is 2 glazes..This one is tempting me to once again experiment with my own mixing!  Nice!
Comment by Catherine Rehbein on May 15, 2011 at 7:15am
Beautiful Glaze effects George! Is this several glazes or just one?
Comment by Sharon Ivy on April 2, 2011 at 10:05pm
I very much like the old, weathered, patina-look on this mug.
Comment by George Lewter on October 9, 2009 at 4:23pm
I don't use any blue, & no cobalt. The blue just arises from the interaction of Floating Red over Waxwing brown. The floating red elicited quite a bit of scorn on the Clayart archives, because it is so low in mainly alumina but also silica, that people said it really isn't a glaze at all! What they are not understanding is the rather magical qualities of Boron. If you think of Gerstely Borate only as a source of flux that point of view holds up. But borates are also glass formers, and are R2O3 components like alumina. I find the glaze reasonably hard, and resistant to acid etching. It goes wildy different colors on the same pot with no other glaze and is quite different over a white body compared to a high iron body - where it goes blue/black where thin.

Recipe Name: Floating Red

Cone: 6 Color: multicolored w iron red
Firing: Oxidation Surface: Glossy

Amount Ingredient
55 Gerstley Borate--1999
15 Talc
30 Silica

100 Total

Additives
15 Iron Oxide--Red

Unity Oxide
.077 Na2O
.323 MgO
.601 CaO
1.000 Total

.112 Al2O3
.587 B2O3
.001 Fe2O3

2.4 SiO2

21.5 Ratio
5.7 Exp

Comments: Note very low alumina and low silica -- low durability
U. Texas Permian Basin recipe. Only recipe I have that has produced a really good iron red.
Fairly runny glaze that produces the reds where it pools the thickest. Best results during a crash cool and a 1 hour hold at 1745F then natural cooling rate. But it also worked fairly well with a slow cool to that temp when I wanted to develop matts in other glazes
Clayart discussions have references to replacing half of the gerstely borate with feldspar. Ive saved that as Floating Red II.
Another suggested variation was to back the GB off to 45 and add 10% EPK. Claimed this kept color and made glaze less runny.
-----------------------------------
Calculations by GlazeMaster™
www.masteringglazes.com
------------------------------------
Comment by Zoophagous on October 9, 2009 at 3:27pm
Very nice. I've never been able to combine an iron red with a blue without it looking awful. What blue are you using?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service